Search results for "Dental veneers"
showing 8 items of 8 documents
A clinical longitudinal study 323 porcelain laminate veneers. Period of study from 3 to 11 years
2009
Objective: The objective of this study was to evaluate the clinical results of 323 porcelain laminate veneers over a period of 3 to 11 years. Material and Methods: This study included 70 patients, aged between 18 and 74 years. Of the 323 total veneers, 124 were of a simple design and 199 were of a functional design. The condition of the soft tissues and hygiene, in addition to the condition of the abutment teeth, the restorations and patient satisfaction were all clinically examined. In carrying out the statistical analysis, a descriptive approach was taken in analyzing the data. The Kaplan Meier method was used for statistically analyzing the survival rates of the porcelain laminate veneer…
An 8-year prospective clinical investigation on the survival rate of feldspathic veneers: Influence of occlusal splint in patients with bruxism
2020
Este artículo se encuentra disponible en la siguiente URL: https://www.sciencedirect.com/science/article/abs/pii/S0300571220300944?via%3Dihub This is the pre-peer reviewed version of the following article: Faus-Matoses, V., Ruiz-Bell, E., Faus-Matoses, I., Özcan, M., Salvatore, S. & Faus-Llácer, VJ. An 8-year prospective clinical investigation on the survival rate of feldspathic veneers: influence of occlusal splint in patients with bruxism. Journal of Dentistry, vol. 99, art. 103352 (aug. 2020), which has been published in final form at https://doi.org/10.1016/j.jdent.2020.103352 Este es el pre-print del siguiente artículo: Faus-Matoses, V., Ruiz-Bell, E., Faus-Matoses, I., Özcan, M., Salv…
Bond strength evaluation of the veneering-core ceramics bonds.
2009
The purpose of this study was to determine whether the bond of veneering porcelain to a ceramic core in bilayered ceramics was similar to that of the metal ceramic control of well known behaviour. Six groups of nine specimens each were fabricated, whose dimensions were 15 mm long and 8 mm in diameter at the core, and 2 mm long and 8 mm in diameter for the veneer. The groups were GR. 1 (control group): CrNi alloy/d.SIGN (Ivoclar), GR. 2: IPS e.maxPress/IPS e.maxCeram (Ivoclar), GR. 3: IPS e.maxZirCad/ IPS e.maxZirPress (Ivoclar), GR. 4: IPS e.maxZirCad/IPS e.maxCeram (Ivoclar), GR. 5: Lava Frame (3M ESPE)/ Lava Ceram (3M ESPE) and GR. 6: Lava Frame (3M ESPE)/IPS e.maxCeram (Ivoclar). A shear…
Influence of bruxism on survival of porcelain laminate veneers
2013
Objectives: This study aims to determine whether bruxism and the use of occlusal splints affect the survival of porcelain laminate veneers in patients treated with this technique. Material and Methods: Restorations were made in 70 patients, including 30 patients with some type of parafunc - tional habit. A total of 323 veneers were placed, 170 in patients with bruxism activity, and the remaining 153 in patients without it. A clinical examination determined the presence or absence of ceramic failure (cracks, frac - tures and debonding) of the restorations; these incidents were analyzed for association with bruxism and the use of splints. Results: Analysis of the ceramic failures showed that …
A prospective evaluation of zirconia anterior partial fixed dental prostheses: Clinical results after seven years.
2014
Abstract Statement of problem Because of the high mechanical strength of zirconium dioxide, the metal in fixed partial prostheses can now be replaced. However, the material is susceptible to aging or hydrothermal degradation and to chipping of the feldspathic veneer. Purpose The purpose of this prospective study was to evaluate the survival (without failure) and success (survival without any complication or failure) rate and clinical efficacy of anterior zirconia partial fixed dental prostheses. Material and methods Twenty-seven anterior partial fixed dental prostheses of 3 to 6 units were fabricated. All participants were examined after 1 month and 6 months, then annually for 7 years. Resu…
Comparative fracture behavior of monolithic and veneered zirconia posterior fixed dental prostheses
2017
The purpose of this study was to evaluate and to compare the fracture load and the fracture pattern of monolithic and veneered zirconia posterior fixed dental prostheses (FDPs). Twenty standardized steel dies were prepared to receive posterior 3-unit FDPs. Specimens were randomly divided into 2 groups (n=10): (1) Lava Zirconia, and (2) Lava Plus. All FDPs were cemented using glass ionomer cement and subjected to thermal and mechanical cycling at 5-55ºC with a 30-s dwell time for 120,000 masticatory cycles. All specimens were subjected to a three-point bending test until fracture. Data were statistically analyzed using Student's t test, paired t-test and Weibull statistics (α=0.05). No diffe…
Effect of Thermomechanical and Static Loading on the Load to Fracture of Metal‐Ceramic, Monolithic and Veneered Zirconia Posterior Fixed Partial Dent…
2018
PURPOSE To evaluate the influence of static (not preloaded) and thermomechanical loading on the load to fracture of metal-ceramic, monolithic and veneered zirconia computer-aided design/computer-aided manufacturing (CAD/CAM) posterior fixed partial dentures (FPDs). MATERIALS AND METHODS One hundred standardized specimens with 2 abutments screwed onto a platform were prepared from stainless steel to receive a posterior 3-unit FPD with an intermediate pontic. Specimens were randomly divided into 5 groups (n = 20): Metal-ceramic (control group), Lava Zirconia system, Vita In-Ceram YZ, IPS e.max ZirCAD, and Lava Plus. Half of the specimens of each group (n = 10) underwent no preloading, and the…
Clinical outcomes of veneered zirconia anterior partial fixed dental prostheses: A 12-year prospective clinical trial
2019
Abstract Statement of problem Anterior veneered zirconia partial fixed dental prostheses (FDPs) have substituted for metal-ceramic to improve esthetics and biocompatibility. However, the material is susceptible to aging or hydrothermal degradation and to chipping of the feldspathic veneer. Whether these susceptibilities limit the clinical performance of anterior veneered zirconia FPDs is unclear. Purpose The purpose of this prospective clinical study was to analyze the mechanical and biologic behavior of zirconia partial FDPs in the anterior region over a 12-year follow-up period. Material and methods Twenty-seven 3- to 6-unit FDPs fabricated from zirconia veneered with feldspathic porcelai…